- Indonesia
NIVOPLAN
Application | : | Smoothing walls prior | Repairing old, damaged renders | Levelling reinforced concrete surfaces | Smoothing foamed cement, brick, eraclit, etc. walls |
Colour | : | White | Grey |
Consistency | : | Powder |
Consistency Of Mix | : | Very pasty |
Flooring | : | Flooring | Walling |
Material | : | Concrete |
Product type | : | Admixture |
Usage | : | Interior | Exterior |
Thickness possible | : | For One CoatFrom 2 to 20 mm |
Weight | : | 25 kg |
Application Temperature Range | : | From +5°C to +30°C |
Bond Strength On Brickwork | : | Not required | ≥ 0.8 FP: B |
Compatibility With Adhesives | : | Excellent |
Compressive Strength | : | ≥ 12 category CS IV (MPa) | ≥ 6 category CS IV (MPa) | 6.0 N/ mm² |
Density | : | 1.400 kg/ m³ |
Density Of Mix | : | 1.830 kg/ m³ |
Dry Solids Content Or Active Substance | : | 100 % |
Flexural Strength | : | 3.5 N/ mm² |
Mix Ratio | : | 23 - 26 parts water per 100 parts of Nivoplan by weight |
pH Of Mix | : | Approx. 12 |
Pot Life | : | 2 - 3 hours |
Resistance To Alkalis | : | Excellent |
Resistance To Oils | : | Excellent (poor to vegetable oils) |
Resistance To Solvents | : | Excellent |
Storage | : | 12 months |
Temperature Range When In Use | : | From –30 °C to +90 °C |
Thermal Conductivity -λ- | : | Not required | 0.95 (W/m·K°) |
Waiting Time Before Bonding | : | > 24 hours dependant on thickness and temperature |
Waiting Time Before Painting | : | At least 14 days |
Water Absorption | : | W0 (not specified) | W1 (≤ 0.40) | W2 (≤ 0.20) |
Bond Strength On Brickwork Certification | : | EN 1015-12 |
Coefficient Of Vapour Permeability Certification | : | EN 1015-19 |
Compressive Strength Certification | : | EN 1015-11 |
Thermal Conductivity -λ- Certification | : | EN 1745 |
Water Absorption Certification | : | EN 1015-18 |